| 性能項目 | 試驗條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | |
| 基本性能 | 吸水率 | --- | ASTM D-570 | 0.15 | % |
| 物理性能 | 比重 | --- | ASTM D-792 | 1.2 | --- |
| 阻燃性 | 1/6"英寸 | UL 94 | V-0 | --- | |
| 模具收縮率 | 3mmt | ASTM D-955 | 0.5~0.7 | % | |
| 機械性能 | 拉伸強度 | --- | ASTM D-638 | 680 | Kg/cm2 |
| 斷裂伸長率 | --- | ASTM D-638 | 150 | % | |
| 彎曲強度 | --- | ASTM D-790 | 900 | Kg/cm2 | |
| 彎曲模量 | --- | ASTM D-790 | 21500 | Kg/cm2 | |
| IZOD沖擊強度 | 1/8"英寸 | ASTM D-256 | 75 | kg?1?79?1?79cm/cm | |
| 洛氏硬度 | --- | ASTM D-785 | 120 | R scale | |
| 電氣性能 | 體積電阻率 | 1016 | ASTM D-257 | 4 | Ω.cm |
| 介電強度 | --- | ASTM D-149 | 30 | KV/mm | |
| 導電率 | 1016Hz | ASTM D-150 | 2.85 | --- | |
| 損耗因素 | --- | ASTM D-150 | 0.0092 | --- | |
| 耐ARC性 | --- | ASTM D-495 | 120 | sec | |
| 熱 性 能 | 熱膨脹系數(shù) | --- | ASTM D-696 | 5.6×10-5 | mm/mm/℃ |
| HDT熱變形溫度 | 4.6kg/cm2 | ASTM D-648 | 145 | ℃ | |
| HDT熱變形溫度 | 18.6kg/cm2 | ASTM D-648 | 134 | ℃ | |
PC/韓國三星/EN-1052/無鹵阻燃V0/耐高溫/高流動